Products · The last 4%

Mulch, fiber & biomass

Some wood is genuinely finished. Rather than bury it, we grind it: landscape mulch, animal bedding, erosion control, boiler fiber. This is the line that makes 'zero to landfill' a fact instead of a slogan.

Start a request on this page

Twelve seconds of typing beats a week of phone tag. Everything you send lands with a coordinator who knows the yard inventory.

Grind sizes
3 standard screens
Bulk minimum
10 cubic yards
Delivery radius
60 miles
Dye
Iron-oxide, optional
A working business address — we reply here, and only here.
US or Canada only. Area code + 7 digits — we format it as you type.
US ZIP (78728 or 78728-1234) or Canadian postal code (M5V 2T6). It must match the state.
Whole units, 1 to 1,000,000. Use the message field for anything approximate.

Fields marked * are required, and we check them properly — a bad phone number or a ZIP that does not match the state will come back to you. Read our privacy notice.

Mixed stacks of used pallets, including blue-painted ones, on a grass and gravel lot under a grey sky.
Intake, before it is sortedEverything arrives mixed. Sorting it is the first thing we do and the reason grading holds.

Roughly four percent of the wood that enters this yard cannot be a pallet, a crate, a collar or a table ever again. It still does not get buried.

The four streams

ProductScreenGoes toNotes
Landscape mulch1"–2" single grindMunicipal and commercial landscaping, residential bulkNatural, or iron-oxide dyed brown/black
Playground & path fiberDouble grind, screened fines removedTrails, dog parks, arenasNo chemically treated stock, ever
Animal beddingFine grind, HT stock only, kiln driedEquine and livestock operations east of AustinLow dust, tested moisture
Boiler biomassHog fuel, 3" minusIndustrial steam, regional co-genSold by the ton, moisture declared

Why pallet mulch is different from tree mulch

Arborist mulch is mostly bark, leaf and green wood: it composts fast, mats down and robs nitrogen while it does so. Pallet mulch is kiln-dry heartwood and sapwood, nail-free after magnetic separation, and already at low moisture. It holds colour longer, knits less, and breaks down slowly — which is exactly what you want in a commercial bed that gets topped once a year rather than three times.

0.0%Landfill across all streamsaudited quarterly
11,400Cubic yards ground last yearfrom this yard alone
3Magnetic separation passesbefore any grind leaves

Buying it

  • Bulk, delivered — 10 yard minimum inside 60 miles of 78728, walking-floor or dump trailer.
  • Bulk, loaded — bring a trailer to the yard; we load during yard hours including Saturday mornings.
  • Bagged — 2 cubic foot bags, pallet quantities only (and the pallet is, naturally, recycled).
  • Standing landscape contracts — scheduled drops through the season, priced annually.
Are there nails in it?

Three magnetic separation passes, and a hand inspection of the finished windrow. Our playground and bedding grades are additionally screened. We have never had a nail claim on bedding stock, and we would tell you if we had.

Is it safe around vegetable gardens?

The natural, undyed mulch from HT stock is. Ask for the HT-only designation on the ticket and we will segregate the load.

Can you take our wood waste?

Often, yes — clean wood only, no engineered panel, no painted or treated lumber. Ask about a recycling pickup.


Specification appendix

The reference tables behind everything above, in one place. These are the same figures our own benches and coordinators work from, and the same ones we will put in a written grading standard for your account.

Every footprint we stock

FootprintInchesMillimetresConstructionWhere it livesOur stockPer 53' van
GMA 48×4048" × 40"1219 × 1016Stringer & blockGrocery, general distribution, retailDeep480–560
48×4848" × 48"1219 × 1219StringerDrums, reels, wire, square loadsGood392–420
48×4548" × 45"1219 × 1143StringerAutomotive, tyreGood420–450
48×4248" × 42"1219 × 1067StringerTelecom, paint, coatingsGood440–480
42×4242" × 42"1067 × 1067StringerChemicals, drums, paintGood480–520
40×4840" × 48"1016 × 1219StringerBeverage, rotated GMAGood480–560
40×4040" × 40"1016 × 1016StringerDairy, beverage, bakeryGood520–580
36×3636" × 36"914 × 914StringerCompact, display, light goodsGood640–700
32×3032" × 30"813 × 762StringerRetail display, in-storeLimited900+
30×3030" × 30"762 × 762StringerLight goods, displayLimited960+
48×20 half48" × 20"1219 × 508StringerRetail half pallet, promotionsLimited1,000+
EPAL 147.24" × 31.50"1200 × 800Block, 9 blocksEuropean trade, retailTo order540–600
EPAL 2 / ISO47.24" × 39.37"1200 × 1000BlockEurope, Asia, best container fitTo order480–520
Asia square43.30" × 43.30"1100 × 1100BlockJapan, east AsiaTo order460–500
AU square44.88" × 44.88"1140 × 1140BlockAustralia, chemical CP seriesTo order440–480

Trailer counts are for stacked, unstrapped loads of sound recycled stock and vary with repair thickness. We confirm the actual count on the bill of lading rather than estimating it. Anything not on this list we cut from reclaim — see custom milling.

Grades, side by side

Grade AGrade B#1 premium#2 economyCustom cut
Original boardsAllSome replacedAllSeveral replacedMixed
Companion boardsNonePermittedNonePermittedPermitted
Stringer plugsNonePermittedNonePermittedPermitted
Metal platesNonePermitted, disclosedNonePermittedPermitted
SquarenessWithin ¼"Within ½"Within ¼"Within ½"Within ½"
Colour uniformityHighMixedHighMixedMixed, fresh saw ends
Protruding fastenersZeroZeroZeroZeroZero
Moisture ceiling19% (15% on request)19%19% (15% on request)19%19%
Typical serviceRetail-facing, exportInternal, bulkAutomation, rackingOne-way, yard storageOdd footprints
Relative priceHighest recycled−18 to −30%HighLowest≈⅓ of a new build
Remaining lifeLongestShorter — already repaired onceLongestShortestVaries

Grade A and #1 overlap: we use #1 for units that needed no repair at all and A for units that are cosmetically uniform. Where a customer holds their own written standard, that document governs and supersedes these names.

Load ratings and unit weights

ConstructionStaticDynamicRacked (unsupported)Unit weight
Recycled GMA 48×40 stringer, sound4,600 lb2,800 lb1,500 lb33–45 lb
Recycled 48×40 block, sound5,200 lb3,000 lb1,900 lb40–55 lb
Recycled 48×40 stringer, repaired (B)4,400 lb2,650 lb1,400 lb35–48 lb
New southern yellow pine, 5 top boards4,200 lb2,500 lb1,400 lb33–38 lb
New mixed hardwood block, 7 top boards6,000 lb3,500 lb2,400 lb48–58 lb
Heavy-duty new build, doubled stringers9,000 lb5,000 lb3,800 lb62–78 lb
Skid (no bottom deck)3,800 lb2,200 lbNot for racking24–32 lb

Representative planning figures for sound stock, not engineering certifications. Racked ratings assume the load spans two rails with nothing under the middle. Derate a further 20–30% for dwell times beyond a few weeks, because wood creeps under sustained load.

  • Design ceiling: deflection of span ÷ 100 — about 0.4 inches across a 40-inch unsupported span.
  • Orientation: rack a stringer pallet across the wrong axis and the deck boards carry the span instead of the stringers. Capacity can halve.
  • Creep: wood deflects progressively under sustained load. A unit measured inside tolerance on day one can exceed it after six months in a rack.
  • Stiffness, not strength, is the limit. Mixed hardwood outperforms southern yellow pine in racking by more than their strength figures suggest, because it is substantially stiffer.
  • Drive-in racking gives a long unsupported span with no support at the leading edge. Derate hard, use block construction, consider full-perimeter bottom boards.

Tolerances that get argued about

Overall footprint
±¼" is normal in recycled stock. ±⅛" is achievable on new builds and worth paying for only if you run automation.
Squareness
Diagonal difference under ½". Beyond that, racking and ASRS reject it, and stretch wrap tightens on two corners and slackens on the other two.
Deck gap
Typically 3½" between boards. Conveyor lines often need a maximum of 3". Specify the number in inches — it is not implied by a grade.
Entry height
Nominal 3½". A repair with thicker boards can lose ¼" and still look fine, then wedge a powered pallet jack.
Board thickness
Nominal ⅝" may measure 0.60–0.66". Specify a minimum if deck flatness matters to your product.
Protruding fasteners
Zero tolerance. Any nail standing above the deck surface condemns the unit at our bench.
Moisture content
19% is the mould threshold and our standard ceiling. 15% on request for food contact and chilled service.
Bark
Some export destinations require debarked wood. Ask before you load, not after.

Species and what each one is good for

SpeciesRelative densityStiffnessNail holdingWeightWhere we use it
Mixed hardwood (oak, maple, gum, hickory)HighHighestExcellentHeaviestRacked service, stringers, blocks, bedding feedstock
Red / white oakHighHighExcellentHeavyHeavy-duty stringers, furniture stock
Southern yellow pineMediumMediumGood for a softwoodLightNew builds, floor-stored service, crate framing
PoplarLow–mediumLowModerateLightCollar panels, crate sheathing, light decks
Spruce / fir (inbound EU & Canadian units)LowLowModerateLightestArrives on imported pallets; harvested for light components
Mixed reclaim (unknown)VariesVariesVariesVariesGraded on behaviour, never on a species claim

A single Grade B recycled pallet can contain four species in no reliable proportion, which is why we grade on inspection rather than on a species label. Where stiffness genuinely matters, specify mixed hardwood — it is the cheapest real structural upgrade available.

Fasteners

FastenerHow it holdsRelative withdrawalCorrect forWrong for
Ring (annular) shankRings bite into the fibre; withdrawal must tear wood1.8–2.2Deck boards, repairs, anywhere a fork strikes—
Helical (screw) shankThreads itself into the fibre as it drives1.7–2.1Stringers, blocks, hardwood—
Smooth shankFriction only; wood shrinks away from it1.0 (baseline)Nothing in a palletEvery pallet joint
StaplesTwo thin legs, wide crown, large bearing area0.5–0.8Collar panels, crate sheathing, lidsDeck and stringer joints
Galvanised (any shank)As above, corrosion resistantAs aboveOutdoor and wash-down service—

Doubling withdrawal resistance roughly doubles the number of trips a unit survives, for a fastener cost measured in cents. We use ring-shank and helical only, and every unit that has been apart is fully re-nailed. The MIBANT bend-angle test is the industry's rough proxy for nail ductility: too brittle and it snaps on impact, too soft and the joint loosens.

Moisture

Moisture contentWhat happensTypical sourceFreight weight
6–12%Indoor equilibrium. No mould risk. Dimensionally stable.Kiln dried, stored insideLightest
12–19%Safe working range — our standard ceiling.Covered dry stackNormal
19–25%Mould within days to weeks in warm conditions.Rain-exposed stacks, green lumber+5–10%
25–40%Mould rapid, blue stain likely.Pallets left in the open through a wet week+10–20%
Above 40%Saturated. You are paying freight on water.Standing water, flooded yard+20%+

Mould needs free water. Below roughly 19% the water in wood is chemically bound in the cell walls and spores cannot germinate; above it, they can. Heat treatment kills insects and confers no moisture guarantee; kiln drying reduces moisture and is not a phytosanitary treatment. They are separate claims and conflating them causes both mould claims and border holds.

How to specify, in ten lines

  1. Footprint, length first, in inches — and the carton pattern that produced it, so we can check for overhang.
  2. Construction: stringer or block, two-way or four-way entry. Specify block if you cannot control racking orientation.
  3. Maximum deck gap in inches. This is the number that decides whether a carton falls through your rollers, and no grade implies it.
  4. Minimum entry height if you run powered pallet jacks. Repairs with thicker boards quietly eat clearance.
  5. Squareness tolerance. ±¼" for racking and automation; ±½" is fine for floor storage and cheaper.
  6. Moisture ceiling, with the measurement method named. 19% standard, 15% for food contact or chilled service.
  7. Treatment: HT and ISPM-15 marked, and re-marked after any repair introducing untreated wood.
  8. Species, if stiffness matters. Mixed hardwood for racked service; southern yellow pine where nothing spans anything.
  9. Permitted repairs: plates allowed or not, companion boards allowed or not. Automation usually wants neither.
  10. Load case: weight, support condition, dwell time, whether it stacks. This is what lets us pick the grade rather than you guessing it.

Standards, testing and defects

What governs this trade, how pallets are actually tested, and the defect list our benches work from. Published because a specification you can check is worth more to us than a lead we captured.

The documents that govern wood packaging

DocumentIssued byWhat it governsDoes it bind us?
ISPM-15IPPC / FAOPhytosanitary treatment and marking of solid wood packaging crossing bordersYes — we are a registered treating facility
ISO 6780ISOThe six recognised pallet footprints for international tradeReference; we stock four of the six
ISO 8611-1/2/3ISOTest methods, performance requirements and maximum working loads for flat palletsMethods we quote; we do not issue certifications for recycled stock
ISO 18613ISORepair of flat wooden palletsOur bench practice aligns with it
ASTM D1185ASTMStandard test methods for pallets and related structuresReference for new-build testing
ASTM D6179ASTMRough handling of unitised loads — incline impact, drop, vibrationReference for unit-load advice
MIL-STD-1660US DoDDesign criteria for ammunition unit loadsOnly on defence-adjacent work, by request
GMA specificationGrocery Manufacturers Association (historic)The 48×40 footprint, board count and notch geometryThe de facto North American default
NWPCA uniform standardNational Wooden Pallet & Container AssociationRecycled pallet grading vocabularyYes, unless a customer standard supersedes it
EPAL technical regulationsEuropean Pallet AssociationLicensed manufacture and repair of EUR/EPAL palletsNo — we hold no EPAL licence and say so
NHLA rulesNational Hardwood Lumber AssociationHardwood lumber gradingUpstream of us; pallet stock sits below the appearance grades
ANSI MH1ANSI / MHIPallets, slip sheets and other material handling definitionsTerminology reference

We list what does not bind us as deliberately as what does. A supplier vague about which standards it actually holds is the main avoidable risk in this trade.

Test methods and what each one tells you

TestWhat it simulatesWhat it tells youWhere it matters
Compression, edge-supportedRacking across two railsRacked working load and deflectionThe binding constraint in most warehouses
Compression, floor-supportedA load sitting on a flat floorStatic capacity — the biggest and least useful figureFloor storage only
Bending, fork-supportedLifting on forksDynamic capacityEvery movement
Incline impact (conbur)Railcar coupling and hard brakingWhether the unit load stays togetherRail and long-haul road freight
Vibration, random and fixed-frequencyHours of road or rail travelFastener loosening and load settlementLong lanes; this is what kills smooth-shank nails
Drop and corner dropDock mishandlingLead board and corner survivabilityHigh-touch distribution
Fastener withdrawalJoint failure under cyclingService life more than anything else doesEvery pallet, every time
Creep / sustained loadMonths in a rackLong-term deflection; derate 20–30%Slow-moving stock, bagged goods
Moisture determinationStorage realityMould risk and freight weightAll food, chilled and humid-climate work

We publish tested figures for new builds and representative figures for recycled stock. Every unit of reclaim has an individual history, so an engineering certification on recycled wood would imply a precision nobody can hold.

Defects, severity and what we do about each

DefectWhere it showsSeverityWhat our bench does
Lead board split lengthwiseOutermost top board, either endLowBoard swap. Commonest repair in the trade; usually means a steep dock leveller
Interior deck board crackAny top or bottom boardLowBoard swap, or companion board where removal would damage the stringer
End-grain separationBoard end, at the nail lineTerminal for that boardBoard removed and harvested short, or ground. It predicts the next failure
Stringer crack, not crossing a notchOuter or centre stringerMediumPlug if over a third of the depth; otherwise re-nail and pass
Stringer crack crossing a notchAt a notch cornerHighPlug or condemn. The load path through that stringer is gone
Protruding fastenerAnywhere on the deckZero toleranceDriven or replaced before the unit leaves, no exceptions
Loose joint / creakWhole unitMediumFull re-nail. A creaking pallet has already failed at the joints
Missing chamferBottom board lead edgeMediumRe-chamfer. Without it every pallet jack fights the unit
Out of square beyond ½"DiagonalsMedium–highCorrected or condemned. Racking, ASRS and stretch wrap all reject it
Moisture above 19%Whole unitHighDry stack or kiln before repair. Mould is then a question of time
Blue stain / sapstainSapwood facesCosmetic, plus odourRejected for food and absorbent product; fine elsewhere
Bark / waneBoard edgesLow, unless exportRemoved where a destination requires debarked wood
Mould, visibleAny surfaceRejectNever shipped to a food account; dried and re-graded or ground
Paint, stain, coatingAny surfaceRejectSegregated at the gate; industrial fuel stream only
Oil or chemical contaminationAny surfaceRefusedRefused at the gate and the customer is told why
Embedded metal beyond fastenersAnywhereHighRemoved by hand before any grind; it destroys knives

Fastener specifications

FastenerTypical lengthWire gaugeMIBANT bend angleUsed in
Helical, hardened2¼"–2½"0.099–0.120"10–20°Stringers and blocks, hardwood
Helical, standard2"–2¼"0.099–0.113"20–30°Stringers in softwood
Ring shank, hardened1¾"–2¼"0.099–0.113"15–25°Deck boards, repairs
Ring shank, standard1½"–2"0.092–0.105"25–35°Deck boards, lighter stock
Ring shank, galvanised1¾"–2¼"0.099–0.113"20–30°Outdoor and wash-down service
Staple, crown1¼"–1¾"16–15 gaugen/aCollar panels, crate sheathing, lids
Smooth shankanyanyanyNothing we build

A lower MIBANT angle means harder, more brittle steel — better withdrawal, more prone to shearing on impact. A higher angle means softer steel that bends rather than snapping, and joints that loosen. Pallet builders pick a window; cheap builders pick a price. 60 to 78 fasteners go into a standard GMA unit.

Commercial appendix

The arithmetic behind a pallet decision, the sector matrix, and the four decision trees we walk customers through.

Cost per trip, worked

LineOne-way recycledRepaired recycled, 6 tripsNew build, 10 tripsPooled rental
Unit cost delivered$11.50$13.00$26.00$0 capital
Useful trips1610per trip
Cost of the asset per trip$11.50$2.17$2.60$5.50 issue fee
Freight per trip$1.80$1.80$1.80included
Repair share per trip—$0.55$0.42included
Handling labour per trip$0.90$0.90$0.90$0.90
Loss / non-return per tripn/a$0.30$0.75$2.10–6.00
Disposal$0.40creditcreditn/a
Cost per trip$14.60$5.72$6.47$8.50–12.40

A worked illustration using mid-2020s Central Texas figures, not a quotation. The decisive line is loss: pooling and new builds are both excellent until units stop coming back, and the pooled range above reflects return rates between 90% and 55%. Model your own return rate before you model anything else.

Building your own model

  1. Delivered unit cost. Not the quoted unit price — add the freight to your dock.
  2. Useful trips per unit. Ask your supplier, then halve it until you have your own data.
  3. Return rate. Of units leaving your building, how many come back into your control? Operations assume 80% and discover 45%.
  4. Repair cost and repair rate. What share needs work per cycle, and at what price.
  5. Handling labour. Count touches, multiply by minutes, multiply by fully loaded labour cost.
  6. Disposal or credit. A yard that pays for broken units turns this line from a cost into revenue.
  7. Failure cost. Rare, expensive, and the reason cheapest-per-unit is not cheapest-per-trip.
  8. Then divide. Total cost ÷ useful trips. That is the only number worth negotiating on.

What each sector actually needs

SectorUsual footprintUsual gradeThe spec that matters mostFailure that costs most
Grocery & retail distribution48×40A / #1Deck gap and appearanceRejection at a retail DC door
Food manufacturing48×40A / #1Moisture ≤15%Mould transfer to packaging
Beverage48×40, 40×48A / BRacked rating, deck strengthRack deflection under dense load
Construction & building supply48×40, 48×48B / #2Racked rating, outdoor creepRack incident under bagged goods
Agriculture & produce48×40, binsB, HT onlyVentilation, treatment segregationChemically treated wood near feed
Chemicals & paint42×42, 48×48A / BSquare footprint, drum stabilityDrum shift in transit
Automotive48×45, customA / newTolerance, returnable designLine stoppage
Pharmaceutical48×40, newNew / plasticDocumented custody, cleanabilityAudit failure
3PL & warehousingMixedPer clientAsset tracking, written standardsUnbilled pallet leakage
Manufacturing & electronicsCustom, 48×40A / #1 / newSquareness, entry heightASRS rejection, jammed jack
Export & freight forwardingDestination'sB + HTISPM-15 truthContainer held on a quay
Hospitality & events48×40, halfB / #2Collection frequencyService corridor blocked

Decision trees

Recycled, new, or cut down?

  1. Does a standard footprint fit your carton pattern with no overhang? If yes → recycled.
  2. If no: does an oversized footprint exist in reclaim that can be sawn to your size? If yes → cut down, at roughly a third of a new build.
  3. Does anything automated read the pallet's geometry, or do you need ±⅛"? If yes → new build.
  4. Is the racked load above about 2,500 lb? If yes → new build, mixed hardwood, block construction.
  5. Is a documented chain of custody for the wood itself part of an audit? If yes → new build.
  6. Otherwise → recycled, at the lowest grade that survives the journey.

Buy, own a fleet, or rent from a pool?

  1. Measure your return rate first. Everything below depends on it and nothing else matters as much.
  2. Below 50% return → your pallet is packaging. Buy recycled one-way and price it as consumable.
  3. 50–85% return → the messy middle. Buy recycled on a managed programme, with collection on the same movements.
  4. Above 85% return, with controlled geography → own a fleet and use toll repair to keep your asset numbers.
  5. Mandated by a retailer's pool, or shipping to hundreds of points needing identical quality → pool rental, and budget for loss charges.
  6. Wash-down hygiene is a process requirement → plastic, and we will point you to somebody who sells it.

Stringer or block?

  1. Does it go into racking where you cannot guarantee orientation? Block.
  2. Do powered jacks enter from the 48" side? Block.
  3. Automated storage and retrieval? Block, or new.
  4. Heavy load sitting for months? Block, mixed hardwood.
  5. European or ISO-metric footprint? Block by specification, not preference.
  6. Otherwise → stringer: lighter, cheaper, deeper in recycled stock and easier to repair.

Repair or replace?

  1. Crack crossing a notch, or more than a third of a stringer's depth? Plug, or condemn.
  2. Three or more stringer repairs already present? Condemn — that is a pallet held together by optimism.
  3. Four or more deck boards gone on a low-value footprint? Harvest the boards.
  4. Above 24% moisture? Dry stack first, then decide.
  5. Contaminated with oil, chemicals or paint? Out of every reuse stream, permanently.
  6. Otherwise → repair and re-nail fully, at roughly a third of replacement cost.
Get a quoteFull form · no phone needed